Featured

SL38 CIVIL ENGINEERING MCQ AND SHORT TYPE QUESTION ANSWER

STUDY LESSON:-38 [CIVIL ENGINEERING]
For Competitive exams/Govt. jobs/Semester exam/Self Study Purpose


 1. Due to the presence of excess carbonaceous matter and sulpher in brick clay the defect observed is called ________ 
2. The black core in brick work causes due to the presence of ________

3. Lime used for plastering are usually __________

4. Knots are the weakness of ________ when it is subjected to compression
    a) steel     b) timber     c) concrete     d) none of these

5. The increase in volume of a concerned mass of a sand caused by the presence of moisture is known as 
    a) Efflorescence     b) Shrinkage     c) Bulking     d) Swelling 

6. Heart shake, Wane, Ringdall, Brown rot these are the types of __________

7. The minimum strength of a common building bricks should be_________
     a) 2.5 Mpa    b) 3 Mpa     c) 3.5Mpa     d) 4Mpa

8. Efflorescence in a brick surface is caused by the presence of __________ 

9. A good brick earth should contain ________ of silica.
    a) 20 to 30%     b) 40 to 50%     c) 50 to 60%     d) 70 to 80%

10. _________ acts as a flux in the klin during burning and they causes the bricks to fuse, twist and wrap.



Answers:-
1.Bloating
2. bituminous matter and carbon
3. Fat lime or hydraulic lime
4. b) timber  
5. c) Bulking
6. Defects in timber
7. c) 3.5Mpa 
8. Soul-able salts
9. c) 50 to 60%
10. Alkalies

author

Civil-Knowledge-Hub Admin

Author Description!

Get Free Email Updates to your Inbox!

Post a Comment